SA662GRC carbon steel plate for medium and low temperature pressure vessels
SA662GRC steel plate corresponding to the GB: 16MNDR European standard: P355NL1
SA662GRC implementation standards: ASTM, ASME standards
ASTM: American Mechanical Association ASME: American Materials Association
National standard: 16MNDR implementation standard: GB/T3531
European standard: P355NL1 implementation standard: EN10025
Heat treatment condition of SA662GRC steel plate: normalizing
Normalizing: The steel plate is heated to an appropriate temperature for cooling in the air
SA662GRC steel plate flaw detection: also known as ultrasonic inspection, is a method of inspection for the internal quality of the steel plate, but also can test the metal internal defects such as (concealed cracks, pores, trachoma and impurities)
SA662GrC中低溫壓力容器用碳鋼板
SA662GrC鋼板對應國標:16MnDR 歐標:P355NL1
SA662GrC執(zhí)行標準:ASTM、ASME標準
ASTM:美國機械協(xié)會 ASME:美國材料協(xié)會
國標:16MnDR執(zhí)行標準:GB/T3531
歐標:P355NL1執(zhí)行標準 :EN10025
SA662GrC鋼板熱處理狀態(tài):正火
正火:將鋼板加熱到適應溫度在空氣中進行冷卻
SA662GrC鋼板可進行探傷:也被稱為超聲波檢驗,是針對鋼板內部質量的一種檢驗方法手段,同時也可以檢驗出金屬內部的缺陷如(隱蔽裂紋、氣孔、沙眼和雜質等)
SA662GrC鋼板化學成分(Wt%)
牌號
化學成分(熔煉分析)%
C:碳
Si:硅
Mn:錳
P:磷
S:硫
ALs:酸熔鋁
SA622GrC
≤0.20
0.15-0.50
1.0-1.6
≤0.035
≤0.04
≥0.020
舞鋼可提供的熱處理(正火、回火、淬火、退火等):
正火:將鋼板加熱到適當溫度在空氣中進行冷卻
回火:將鋼板在某一適當溫度下進行長時間保溫在冷卻
淬火:將鋼板加熱保溫后在水油或其他無機鹽等介質中進行快速冷卻
退火:將鋼板加熱到適宜溫度根據(jù)材料和規(guī)格的不同進行緩慢冷卻